Austenite Stainless Steel

Product Detail

Product Tags

High Temperature Alloy

◆904L can not only solve the general corrosion of sulfuric acid, phosphoric acid and acetic acid, but also solve the problems of chloride pitting corrosion, crevice corrosion and stress corrosion.

◆253Ma (S30815) is a heat-resistant pure austenitic stainless steel developed on the basis of 21Cr-11Ni stainless steel through N alloying and adding rare earth element Ce. It is mainly used in the production of plates.

◆254SMo (F44/S31254) is a very high-end austenitic stainless steel, which is often used as a substitute for high-nickel and titanium alloys. It is mainly used in many corrosive applications such as chemical and petrochemical processes and chloride solutions.

◆Al-6XN(N08367) is suitable for pumps, valves, flanges and piping systems of oil and gas, chemical and electric power.

Chemical composition

Grade

C

Si

Mn

S

P

Cr

Ni

Mo

Cu

N

other

no greater than

904L

0.02

1

2

0.015

0.03

19~21

24~26

4~5

1~2

-

-

253Ma

0.05~0.1

1.4~2

0.8

0.03

0.04

20~22

10~12

-

-

0.14~0.2

Ce0.03~0.08

254SMo

0.02

0.8

1

0.01

0.03

19.5~20.5

17.5~18.5

6~6.5

0.5~1

0.18~0.22

-

Al-6XN

0.03

1

2

0.03

0.04

20~22

23.5~25.5

6~7

≤0.75

0.18~0.25

Alloy property minimum

Grade

state

tensile strength RmN/m㎡

Yield Strength Rp0.2N/m㎡

Elongation As%

Brinell hardness HB

904L

Solution treatment

490

215

35

-

253Ma

Solution treatment

650

310

40

210

254SMo

Solution treatment

650

300

35

-

Al-6XN

Solution treatment

835

480

42

-