IInconel
High Temperature Alloy
◆Inconel600 (N06600) has corrosion resistance to various corrosive media, it also has good creep rupture strength, recommended for the working environment below 700 ℃. It is mainly used in the field of production and use of corrosive alkali metals, especially in environments where sulfides are used.
◆An important performance of Inconel601 (N06601) is that it has oxidation resistance and good carbonization resistance when the temperature is as high as 1180 ° C. It is mainly used in heat treatment processing parts, exhaust system parts, and oxygen reheaters.
◆Inconel625 (N06625Ns336) exhibits excellent corrosion resistance in many media, and the soft annealed low-carbon alloy 625 is widely used in the chemical process industry, where it contacts seawater and withstands high mechanical stress.
◆Inconel725 has strong stress corrosion resistance and is suitable for pipe fittings and marine vessels.
◆Inconel690 has anti-oxidation and anti-corrosion properties, and is suitable for petrochemical, metallurgy, nuclear energy, etc.
Chemical composition
Grade |
C |
Si |
Mn |
S |
P |
Cr |
Ni |
Fe |
Al |
Ti |
Cu |
Mo |
Nb |
other |
no greater than |
||||||||||||||
Inconel600 |
0.15 |
0.5 |
1 |
0.015 |
0.03 |
14~17 |
base |
6~10 |
- |
- |
≤0.5 |
- |
- |
- |
Inconel601 |
0.1 |
0.5 |
1 |
0.015 |
0.03 |
21~25 |
base |
10~15 |
1~1.7 |
- |
≤1 |
- |
- |
- |
Inconel625 |
0.1 |
0.5 |
0.5 |
0.015 |
0.015 |
20~23 |
base |
≤5 |
≤0.4 |
≤0.4 |
- |
8~10 |
3.15~4.15 |
Co≤1 |
Inconel725 |
0.03 |
0.2 |
0.35 |
0.01 |
0.015 |
19~22.5 |
55~59 |
Remain |
0.35 |
1~1.7 |
— |
7~9.5 |
2.75~4 |
- |
Inconel690 |
0.05 |
0.5 |
0.5 |
0.015 |
0.03 |
27~31 |
≥58 |
7~11 |
— |
— |
≤0.5 |
— |
— |
- |
Alloy property minimum
Grade |
alloy state |
tensile strength RmN/m㎡ |
Yield Strength Rp0.2N/m㎡ |
Elongation As% |
Brinell hardness HB |
Inconel600 |
Solution treatment |
550 |
240 |
- |
≤195 |
Solution treatment |
500 |
180 |
- |
≤185 |
|
Inconel601 |
Annealing |
650 |
300 |
- |
- |
Solution treatment |
600 |
240 |
- |
≤220 |
|
Inconel625 |
Solution treatment |
760 |
345 |
- |
≤220 |
Inconel725 |
Solution treatment |
790 |
485 |
28 |
- |
Inconel690 |
Solution treatment |
780 |
450 |
25 |
- |