Incoloy

  • Incoloy

    High Temperature Alloy Chemical composition Grade C Si Mn S P Cr Ni Fe Al Ti Cu Mo other no greater than Incoloy800 0.1 1 1.5 0.015 0.03 19~23 30~35 base 0.15~0.6 0.15~0.6 ≤0.75 — — Incoloy800H 0.05~0.1 1 1.5 0.015 0.03 19~23 30~35 base 0.15~0.6 0.15~0.6 ≤0.75 — — Incoloy800HT 0.06~0.1 1 1.5 0.015 0.03 19~23 30~35 base 0.15~0.6 0.15~0.6 ≤0.75 — Al+Ti   0.85...