High Temperature Alloy

◆Monel400 has excellent corrosion resistance in hydrofluoric acid and fluorine gas, and is suitable for pipe fittings and valves used in chemical industry, petroleum, atomic energy, and marine development.

◆Monel500 has good comprehensive mechanical properties, high strength and good corrosion resistance. It is suitable for fasteners and structural parts used in chemical industry, ships and marine engineering.

◆Monel404 is widely used in petrochemical, nuclear industry, and other cutting-edge industrial components.

Chemical composition

Grade

C

Si

Mn

S

P

Cr

Ni

Mo

Fe

Co

W

Al

Ti

Cu

no greater than

Monel400

0.3

0.5

2

0.024

-

-

base

-

≤2.5

-

-

-

-

28~34

Monel500

0.18

0.5

1.5

0.01

-

-

≥63

-

≤2

-

-

2.3~3.15

0.35~0.85

27~33

Monel404

0.15

0.1

0.1

0.024

52~57

≤0.5

≤0.05

Remain

Alloy property minimum

Grade

Technical conditions

tensile strength RmN/m㎡

Yield Strength Rp0.2N/m㎡

Elongation As%

Brinell hardness HB

Monel400

Forged/hot rolled

516

170

35

-

Annealed state

483

170

35

-

Monel500

Forged state + aging

960

686

20

27

solid solution + aging

896

585

20

24

Monel404

Annealed state

550

185

36

-