Nickel

Product Detail

Product Tags

High Temperature Alloy

◆Nickel200 is a pure commercial (99.6%) made of nickel, which has excellent mechanical properties and excellent corrosion resistance, high thermal and electrical conductivity, low gas content and low vapor pressure.

◆Nickel201 (N02201) is a pure commercial nickel with very low carbon content, it has been approved to serve the environment up to 1230℃.

Chemical composition

Grade

Ni

Fe

Cu

C

Mn

S

Si

Nickel200

99

≤0.4

≤0.25

≤0.15

≤0.35

≤0.01

≤0.35

Nickel201

99

≤0.4

≤0.25

≤0.02

≤0.35

≤0.01

≤0.35

Alloy property minimum

product form

condition

tensile strength RmN/m㎡

Yield Strength Rp0.2N/m㎡

Elongation As%

Brinell hardness HB

stick and strip

hot rolled

60~85

15~45

35~55

45~80

stick and strip

cold drawn or annealed

55~75

15~30

40~55

45~70

plate

annealing

55~80

15~40

40~60

45~75

flakes

annealing

55~75

15~30

40~55

70Highest

Steel Pipe

seamless annealing

55~75

12~30

40~60

70Highest