Nimonic

  • Nimonic

    High Temperature Alloy Chemical composition Grade C Si Mn S P Cr Ni Fe Cu Ti Al Co other no greater than Nimonic90 0.13 1 1 0.015 18~21 base ≤1.5 ≤0.2 2~3 1~2 15~21 lead≤0.002      B≤0.02        Zr≤0.15 Nimonic91 0.1 1 1 0.015 27~30 base ≤1 ≤0.5 1.9~2.7 0.9~1.5 19~21 Nb0.4~1.1  B0.002~0.01  Zr≤0.1 Alloy property minimum Grade state tensile strength RmN/m㎡ Yield Strength Rp0.2N/...